Transparent POlymer or adhesive for quartz
2006-03-14
Aashish Singh
2006-03-14
Matthew Coda
Transparent POlymer or adhesive for quartz
Matthew Coda
2006-03-14
I can't give you specifics but I've looked at the opposite side of this
equation (low dn/dT) and can tell you that what YOU want is to have the
temperature range of interest be above the Tg of your material.
Secondly you'll want something with a high CTE.  You'll have the
greatest dn/dT when you've got a significant volumetric change over your
temperature range of interest.

Good luck,
Matt

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Aashish Singh
Sent: Tuesday, March 14, 2006 1:59 AM
To: [email protected]
Subject: [mems-talk] Transparent POlymer or adhesive for quartz

  Dear All,

  I'm looking for a Transparent Polymer/Adhesive with very large dn/dT,
that can be spin coated over quartz. i have tried popular Norland
Optical adhesive, but its dn/dT is not as large as i want. The
polymer/adhesive we will use at both visible and IR region. The
dispersion curve (variation of R.I with Wavelength) , dn/dT and  low
absorption at the wavelength of operation is important for my
applications.
  Any information and the source form where we can get it will be highly
appreciated.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics