Hi everyone,

Polyimide is a common dielectric material used in micromachined,
planar RF components to reduce coupling between RF signals and lossy
Si substrates. A drawback is the fact that this polymer absorbs water,
causing changes to RF performance with time and environmental
conditions. Does anyone know if the same is true of x-linked SU-8?

Regards,

Michael
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMStaff Inc.