Dear all,

I need to make the hard and smooth transparent polymer coatings on PDMS and
Quartz substrates.
Up to the moment I use one hard siloxane coating (TOKUYAMA TS-56H) with
dip-coating sequence.
This siloxane solution makes the stable smooth layers with a RI=1.46 and
film thickness about 1.0um - 2.5um.
Dose anybody known one of the same products?


Best regards,

Vitali Emelianov

-------------------------------------------------------
caesar research center
Ludwig-Erhard-Allee 2
53175 Bonn Germany

phone:  +49-228-9656-342
fax:    +49-228-9656-9-342
email:  [email protected]
www:   http://www.caesar.de/1677.0.html


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing