Aluminum Thin Film by E-beam Evaporation
2006-07-17
Sreemanth M Uppuluri
2006-07-17
pradeep # sharma
2006-07-17
Michael D Martin
Aluminum Thin Film by E-beam Evaporation
Sreemanth M Uppuluri
2006-07-17
Hello,

I am trying to obtain very low surface roughness films of Aluminum on Quartz
substrates using e-beam evaporation. Please let me know if there are any
recipes specific to this issue such as speed of deposition, pressure and so
on.

Thanks
Sreemanth


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
MEMS Technology Review
University Wafer