MEMSnet Home: MEMS-Talk: RE: Looking for "Cr evaporation"
RE: Looking for "Cr evaporation"
1998-04-08
Mounir Ennabli
RE: Looking for "Cr evaporation"
Mounir Ennabli
1998-04-08
Dear sir
I haven't heard about this problem before: the source used for Al should
also fit Cr evaporation.
It is just a matter of calibration of the evaporation system.The system
I use here at MIC is an Alcatel system and the same source is used for
Al and Cr.
regards. Mounir Ennabli

Mounir Ennabli.
Mikroelektronik Centret, byg. 344, rum 154
DTU, DK-2800 Lyngby.
e-mail:[email protected]
Phone:+45 4525 5734

> -----Original Message-----
> From: Cheol-Hyun Han [SMTP:[email protected]]
> Sent: 4. april 1998 05:26
> To:   [email protected]
> Subject:      Looking for "Cr evaporation"
>
> Hi,;
> I'm looking for the way and tools for Chromium(Cr) evaporation.   I'm
> trying to use Al evaporation system in which I used tungsten filament
> with Al wire source.   But I don't know if there wire type Chromium
> source is
> and I can use same machine in our lab. for Al evaporation.
>    If anyone know the source type of Cr and what I can use to
> evaporate
> it(boat or filament), please let me know and any information would be
> welcomed. Thank you.
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing