Glass frit coating, masking, and patterning
2006-09-13
Kagan Topalli
2006-09-13
Brubaker Chad
Glass frit coating, masking, and patterning
Brubaker Chad
2006-09-13
Glass frit is not typically patterned by masking.  It is more commonly
patterned by silk-screening.

Best Regards,
Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel:  480.727.9635, Fax:  480.727.9700  e-mail:
[email protected], www.EVGroup.com

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Kagan Topalli
Sent: Wednesday, September 13, 2006 7:03 AM
To: General MEMS discussion
Subject: [mems-talk] Glass frit coating, masking, and patterning

Hi everbody,
Is there anybody that can advise a reference paper or a book chapter
related
with glass frit coating, masking, and patterning? Could you please also
suggest a company that serves glass frit deposition and patterning?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMStaff Inc.