MEMSnet Home: MEMS-Talk: Nickel wet etching
polyimide
2006-09-26
Yogendra Yadav_04322601
Nickel wet etching
2006-10-18
prabhu arumugam
2006-10-18
Roger Shile
2006-10-18
Hsiu-Jen Wang
Anyone know what this thing called and where to buy it from? Chip carrier? Chip bonding packaging pad?
2006-10-19
Guangchi Archie Xuan
Anyone know what this thing called and where to buy itfrom? Chip carrier? Chip bonding packaging pad?
2006-10-19
Erik Jung
Anyone know what this thing called and where to buy it from? Chip carrier? Chip bonding packaging pad?
2006-10-19
Bill Flounders
Nickel wet etching
Roger Shile
2006-10-18
I usually use Aluminum Etch (phosphoric Acid based) to etch Ni films.  I
believe JT Baker is a supplier.

Roger Shile

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of prabhu arumugam
Sent: Wednesday, October 18, 2006 9:18 AM
To: General MEMS discussion
Subject: [mems-talk] Nickel wet etching

Hello MEMS folks,
can anyone tell me the what we use to etch nickel
films (approx. 30 nm thick)deposited by ebeam and the
supplier.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.