MEMSnet Home: MEMS-Talk: Re: conductive adhesive: cyanoacrylate?
Re: conductive adhesive: cyanoacrylate?
1998-05-20
Joe Shepard
1998-05-20
Rob
1998-05-20
[email protected]
1998-05-20
Emilio P. Calius
1998-05-21
Gordon Couger
1998-05-21
Samuel E. Riffle
1998-05-23
bob lyness
Re: conductive adhesive: cyanoacrylate?
Emilio P. Calius
1998-05-20
At 21:24 14/05/98 -0400, you wrote:
>I am an industrial manufacturer seeking a conductive adhesive.
>...
>Does anyone know of a similar commercially available conductive
>adhesive?  Or even a two-part conductive epoxy?
>

I have succesfully used Circuit Works CW-2400 2-part conductive epoxy to
install piezoceramic actuator/sensor elements on aluminum beams and plates,
and to connect electrical leads to their electrode surfaces.

This adhesive is manufactured by Chemtronics Inc. in Kennesaw, Georgia (USA)

Dr Emilio P. Calius
Research Engineer: Composite Materials and Structures
Industrial Research Limited
PO Box 2225, Auckland, New Zealand
Ph: +64 9 303 4116,     Fax: +64 9 307 0618


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Addison Engineering