MEMSnet Home: MEMS-Talk: Re: conductive adhesive: cyanoacrylate?
Re: conductive adhesive: cyanoacrylate?
1998-05-20
Joe Shepard
1998-05-20
Rob
1998-05-20
[email protected]
1998-05-20
Emilio P. Calius
1998-05-21
Gordon Couger
1998-05-21
Samuel E. Riffle
1998-05-23
bob lyness
Re: conductive adhesive: cyanoacrylate?
Samuel E. Riffle
1998-05-21
Try  the following, they offer a wide variety of engineering adhesives:

Master Bond, Inc.
154 Hobart Street
Hackensack, New Jersey 07601, USA
Tel: 201-343-8983
Fax: 201-343-2132

Stuart Atwater wrote:

> I am an industrial manufacturer seeking a conductive adhesive.
> Currently I am using superglue, but it seems to wick it way between
> conductive members and cause conducitivity problems.
> Does anyone know of a similar commercially available conductive
> adhesive?  Or even a two-part conductive epoxy?
>
> Thanks,
>
> Stuart Atwater
>

 -
Samuel E. Riffle   [email protected]   401-861-5219  Fax 861-3314
SSRG                http://home.earthlink.net/~sriffle/ssrg/
563 Hope ST, Providence, RI 02906-2603


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Tanner EDA by Mentor Graphics