Hi:

I had the same problem before when I was trying to get a double fixed Cu beam
deposited on silicon substrate. The sacrificed layer was PR. There are two
causes of the sticking. One is the residual stress within the deposited layer
which causes the deformation of the structure, especially when you are using bi-
layer structure. The second is the releasing process. You may want to avoid
using DI water because the surface tension of water may drive the two structures
together during drying. What we did was putting the wafer in alcohol  after
solving the sacrificed layer. And then we put the container into a vaporizing
chamber in room temperature to vaporize all the alcohol, leaving the suspended
structure released. Hope this process can be helpful to your problem.

Yun Wang
Advanced Micro-Nano-Devices Lab
Department of Systems Design Engineering
University of Waterloo, ON, CA
Email:[email protected]

----- Original Message ----
From: deepak agrawal 
To: [email protected]
Sent: Wednesday, January 10, 2007 12:47:16 PM
Subject: [mems-talk] Releasing of the nitride suspended structure

Can i use the dry etching to etch the Aluminum so that there will be no
chance of stiction. Is there anyone has the knowledge about dry etching
recipe of Aluminum.

<>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing