With no success I mean poor etching rate. Do you have a good recipe to suggest a
solution that can give me a rapid deep (> than 10 micrometers) etching pit?

> What do you mean by no success - poor quality or something else? The
> type of glass is also relevant. I have had good results with 2% conc. HF
> + 2% conc. HNO3 when using soda-lime glass. I have never tried it on
> quartz though, but I would not expect it to etch at a similar rate.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
Nano-Master, Inc.
Harrick Plasma, Inc.