Richard,

You might try Ultramet in Pasadena, California.  I do not have
an address for them.  They have definitely performed CVD tungsten
in the past.

-Reid

--
.______________________________________________________________________.
|Reid (Turtle) Alyn Brennen                Hewlett-Packard Laboratories|
|[email protected]                       Chemical Systems Department |
|(650) 857-4469 office                     3500 Deer Creek Road, MS 26U|
|(650) 852-8502 Fax                        Palo Alto, CA 94303-0867    |
`


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMStaff Inc.