Hi,

I have a question regarding dielectric on metal characterization. I
have deposited SiO2 on gold and would like to do an SEM to
characterize the adhesion of the SiO2 to gold but since SiO2 is an
insulator it will charge. Is there another way to characterize the
interface between SiO2 and gold?

Regards,
Leyla Soleymani
University of Toronto
[email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
The Branford Group
Process Variations in Microsystems Manufacturing