Reason for cracks due to high stress in pecvd oxide after annealing
2007-03-11
udaybhaskar katreddi
2007-03-11
Hongzhi CHEN
Reason for cracks due to high stress in pecvd oxide after annealing
udaybhaskar katreddi
2007-03-11
Hi Everybody,
             I have been depositing 1.6 micron silicon dioxide by PECVD process
at 300 degrees temperature on silicon wafer coated with silicon nitride,after
that I am annealing at 620 degrees.Here I am having a problem that the deposited
oxide is peeling off,might be due to high stress ,so someone suggest me some
solution to sortout this problem.

Thankyou and Regards,
Uday.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Addison Engineering
Mentor Graphics Corporation