MEMSnet Home: MEMS-Talk: Pin holes in evaporated Chromium, Titanium and Gold
Pin holes in evaporated Chromium, Titanium and Gold
2007-03-19
Yue Mun Pun, Jeffrey
2007-03-19
Shay Kaplan
2007-03-19
David Casale
2007-03-20
Yue Mun Pun, Jeffrey
Pin holes in evaporated Chromium, Titanium and Gold
Yue Mun Pun, Jeffrey
2007-03-19
Hi,
I'm just wondering if anybody has observed pin holes in thermally or e-beam
evaporated Chromium, Titanium and Gold.  If so, how thick do I have to evaporate
these metal films for the pin holes to disappear?

Mr. Jeffrey Mun Pun YUE
余文彬
Division of Bioengineering
E3A-07-02, Nanobioanalytics Lab
7 Engineering Drive 1
National University of Singapore
Singapore 117574
Tel: (65) 65166482, Fax: (65) 68723069
E-mail:  [email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
The Branford Group