MEMSnet Home: MEMS-Talk: Pinholes in Evaporated Gold film
Pinholes in Evaporated Gold film
2007-03-23
Yue Mun Pun, Jeffrey
Ultra-thin silicon wafers
2007-03-24
Andrea Mazzolari
Pinholes in Evaporated Gold film
Yue Mun Pun, Jeffrey
2007-03-23
Hi,
I am trying to evaporate Gold on uncrosslinked SU-8 film.  Is 100nm a
sufficiently thick layer to block UV light in i-line processing?  Also has
anyone seen pinholes in evaporated gold film?  If so, how thick or what must I
do to avoid pinholes in gold films?

Jeffrey
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
The Branford Group
Process Variations in Microsystems Manufacturing