About Image reversal
2007-04-17
saravan kallempudi
About Image reversal
saravan kallempudi
2007-04-17
Hello,

I am trying to do Liftoff using AZ 5214 E before liftoff  and after baking if I
measured the thickness of the PR, I noticed that there is about 1 micron change
less than what it should be.
I want around 2 micron thick PR @2000 rpm but I am getting around 0.8 to 0.9
micron. For this reason I think I am unable to do liftoff.
Can anyone help me with this.

Thanks in advance
Saravan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
The Branford Group
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation