Re: 100nm coating for E-beam lith (Ren Yang)
2007-05-05
Indusekhar
Re: 100nm coating for E-beam lith (Ren Yang)
Indusekhar
2007-05-05
Helli Ren Yang

Regarding the 100nm commercial resist--You can try with PMMA, EBR-9 HS31 ,
SAL601( -ve resist). IF you need only few plates , you may contact the mask
plate suppliers .

Wish you good luck