Saravan,

Are you curing BCB in the manufacturer's suggested low oxygen oven? We faced
similar problems and bought another oven which purges oxygen from the chamber
before raising the temperature to cure. It seems to fix it.

Deepa

saravan kallempudi  wrote: Hello,

I need spin BCB over patterned Gold, and Nickel.  Well  I am worrying about the
cracks during curing of BCB.
Any suggestions  ?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMS Technology Review