A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Parylene patterning
Parylene patterning
2007-05-24
Leyla Soleymani
2007-05-24
[email protected]
2007-05-24
Leyla Soleymani
Parylene patterning
[email protected]
2007-05-24
Plasma etch and patience can do the job ;).
Various oxygen plasma etch recipes for parylene have been reported (do
eg a quick Google Scholar search on it).
You can use resist as a mask but make sure it's (much) thicker than your
parylene film; you can afterwards wash away the resist with acetone or
your solvent of choice (the parylene will be inert in pretty much any
solvent/etchant). I wouldn't recommend sonicating it though (depending
on how good your parylene adheres to whatever your substrate is).
Cheers,
Dirk


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Leyla Soleymani
Sent: Wednesday, May 23, 2007 11:41 PM
To: General MEMS discussion
Subject: [mems-talk] Parylene patterning

Hi everyone,

Does anyone have any experience with patterning parylene? Can we do
ebeam lithography or phtolothography on this? If so what resist should
be used, how is it supposed to be etched and how is the resist removed
without damaging the parylene?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing