MEMSnet Home: MEMS-Talk: Re: Question on PDMS micro channels
Re: Question on PDMS micro channels
2007-06-19
Bhamidipati srikalyan
2007-06-20
Ciro Chiappini
Re: Question on PDMS micro channels
Bhamidipati srikalyan
2007-06-19
Hi Lai,
PDMS is not compatible with Acetone. Acetone swells PDMS. The structure of
PDMS can be recovered back after evaporating the absorbed Acetone. Alchohols
do swell PDMS to some extent. Ethanol swells PDMS by as much as 3%.
Therefore it is not advisable to use organic solvents in PDMS devices. But,
you can make the surface of the microchannels hydrophilic, so that even
organic solvents can be used in the microchannel.
Regards,
Srikalyan

--
V.S.Sri Kalyan.B
ME, CHemical Engineering,
Indian Institute of Science,
Bangalore-12.
CELL1:9246546995
CELL2:9986704699
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
Addison Engineering