A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Inquiry regarding sidewall deposition of wafers in e-beam metalization
Inquiry regarding sidewall deposition of wafers in e-beam metalization
2007-06-26
polly
Inquiry regarding sidewall deposition of wafers in e-beam metalization
2007-06-26
shay kaplan
Inquiry regarding sidewall deposition of wafersin e-beam metalization
2007-06-26
Bill Moffat
Inquiry regarding sidewall deposition of wafers in e-beam metalization
shay kaplan
2007-06-26
In ebeam evaporation, the process is a line of site process. i.e. the atoms
/ molecules fly on a straight line from the source to the surface. For these
reason, the thickness is proportional to the cosine of the angle. A 90 deg
wall will not get coated. However, in some systems the wafers are tilted and
are rotating during evaporation (planetary fixture). In such a system one
get can some material on the sidewall depending on the system geometry

shay

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of polly
Sent: Tuesday, June 26, 2007 9:58 PM
To: mems_talk
Subject: [mems-talk] Inquiry regarding sidewall deposition of wafers in
e-beam metalization

Dear Sir,

i would like to know if in e-beam metallization, the sidewall (300 micron
thickness face) also get coated with metal(Aluminum). Kindly also refer me
some good tutorial materials in the metalization area.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
The Branford Group
Harrick Plasma, Inc.