MEMSnet Home: MEMS-Talk: Platinum deposition problem
Platinum deposition problem
2007-07-03
sokwon Paik
2007-07-03
Jesse D Fowler
2007-07-03
Jian Wang
2007-07-05
sokwon Paik
articles/case studies Sn Al Cu
2007-07-05
A.E.Reinhardt
2007-07-12
Morten Aarøe
2007-07-05
Michael D Martin
Platinum deposition problem
Michael D Martin
2007-07-05
Another potential complication that we've run into is resist outgassing.
You might want to vacuum bake your substrate before doing the deposition.

-Mike Martin
 U. of Louisville

>>> sokwon Paik  7/5/2007 10:11 AM >>>
Jesse,

  Thank you for your mentoring.

  It was very helpful and made one questions.

  What kind of evaporator you use?

  I tried even lower deposition rate than you and it seems I need to
  use the same machine as you for the platinum coating.

  Thank you,

  Sokwon
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering