MEMSnet Home: MEMS-Talk: germanium etch
germanium etch
2007-09-02
Andrea Mazzolari
2007-09-03
Shay Kaplan
germanium etch
Shay Kaplan
2007-09-03
Hi Andrea,
The best etchants are commercial ones like CR-7 or CR-14, chrome etch 18,
and similar.
They have a long practical shelf life and are good investment.

shay

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Andrea Mazzolari
Sent: Sunday, September 02, 2007 11:04 PM
To: General MEMS discussion
Subject: [mems-talk] germanium etch

Hi all, i need to make etch of germanium.
As etchant i plan to use HNA solution. Here are the steps:

1) deposition of 100nm Cr mask
2) deposition of photoresist s1813 and patterning
3) etch Cr  (???)
4) Germanium etch (HNA).

could someone give me suggestions about a proper etchant which will etch Cr
layer without attack s1813 ?

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
MEMStaff Inc.
Nano-Master, Inc.