TMAH Etching Silicon - loading effects
2007-10-31
Staller, Steven E
2007-11-01
Shay Kaplan
TMAH Etching Silicon - loading effects
Staller, Steven E
2007-10-31
We believe we have observed a strong correlation of <100>:<1111> selectivity to
loading.

When we etch one wafer we get about ½ the selectivity as we do when we etch
25 or more.

Is this a known phenom? Should we expect the selectivity to be effected this
dramatically?

We are talking about selectivities of >65:1 vs ~30:1.

Steve
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
The Branford Group
MEMS Technology Review