Sawtooth Deposition Profile?
2008-03-12
Aaron Datesman
2008-03-12
Kevin Paul Nichols
2008-03-12
Jason Milne
Sawtooth Deposition Profile?
Aaron Datesman
2008-03-12
Dear List Members,

I would like to sputter deposit a metallic film to have a "sawtooth"
thickness profile, shown below:


   /|        /|        /|
  / |       / |       / |
 /  |___/  |___/  |___ etc.

The desired film height is ~100 nm and the width of each feature is ~500
nm.  Can anyone suggest a suitable method to accomplish this?

Regards,

Dr. Aaron Datesman
Materials Science Division
Argonne National Laboratory
9700 S. Cass Avenue
Argonne, IL 60439

(ph) 630-252-9154
(fax) 630-252-9595
[email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.