MEMSnet Home: MEMS-Talk: HELP REQUIRED IN AREA OF ALUMINUM SPUTTERING
HELP REQUIRED IN AREA OF ALUMINUM SPUTTERING
2008-05-19
Nataraj
2008-05-19
Brent Garber
2008-05-19
Andrew Sarangan
2008-05-20
Nataraj
2008-05-19
Ravikumar_Kuppan
2008-05-19
walter
Aluminum sputtering and evaporation
2008-05-20
Sreemanth M Uppuluri
2008-05-20
Gary Hillman
2008-05-20
Shay Kaplan
HELP REQUIRED IN AREA OF ALUMINUM SPUTTERING
Nataraj
2008-05-20
Dear Mr. Brent,

               Thanks for reply, hope the details furnished below is enough
for your analysis

Power Supply :: PULSED DC POWER SUPPLY, Operating at 60 kHz( avl range 50 to
100 )
Power during deposition ::  12 kW ( operating at Power mode )
vacuum @ chamber during sputtering   :: In the range of  2.0 E-03 torr
Substrate ::      PC ( polycarbonate based plastic ) coated with UV curable
paint( Base coat )
We use oil diffusion pumps with Polycold system
Regards,

Nataraj Santhanam

-----Original Message-----
From: Brent Garber [mailto:[email protected]]
Sent: Monday, May 19, 2008 10:40 PM
To: [email protected]; General MEMS discussion
Subject: Re: [mems-talk] HELP REQUIRED IN AREA OF ALUMINUM SPUTTERING

Nataraj,

You will need to provide a little more information as how you are
depositing the aluminum for anyone to help you.

If you are using DC sputtering, I have found the faster the rate the better.

Brent
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
MEMStaff Inc.