MEMSnet Home: MEMS-Talk: BCB cure
BCB cure
2008-06-27
Cassie Iany
2008-06-27
P.E.M. Kuijpers
2008-06-29
Cassie Iany
2008-06-30
Trent Huang
BCB cure
Trent Huang
2008-06-30
Cassie,

What's the substrate and surface films you have underneath the BCB?

Did the BCB change color after the curing process?  There're many
different thermal procedures for the polymer.  What's the EXACT
application baking/curing procedure you used?  (spin rate, softbake,
exposure/development?, stop points, ramping rates, end point, cooling
rate, etc.)

Trent

Cassie Iany wrote:
> Hello,
>
> I am using BCB (dow chemical) 4024-26, after curing in N2 oven, the surface
has very large bubbles which makes the surface looks ugly. Has anybody
encoutered the same problem? Any solution for it?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.