MEMSnet Home: MEMS-Talk: Metal etching
Metal etching
2008-08-06
P.E.M. Kuijpers
2008-08-08
Robert Rehammar
2008-08-13
汪飞
2008-08-07
Jeff Kettle
Metal etching
Robert Rehammar
2008-08-08
Hi Peter,

Two very nice review articles about different etch-rates are by
Williams, K. R. J. of Micromechanincal processing 1996 vol 5 pp 256-269
and Part II by the same person 2003 same journal vol 12 pp 761.

I know there are recipes to etch some or all of these metals. Not sure
about selectivity towards ITO, but maybe somewhere to start.

Regrds,
Robert

ons 2008-08-06 klockan 08:06 +0200 skrev P.E.M. Kuijpers:
> Dear all,
>
> Can one of these metals  Cr, Ti, Cu or Mo selectively be etched compared to
> ITO and what kind of etchant can be used for this
>
> Thanks
> Peter
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.