2008-09-15
Ken Healy
2008-09-15
Shay Kaplan
2008-09-15
Koray Karakaya
2008-09-16
Ken Healy
Under what conditions is buffered-HF (BOE) etching diffusion limited?
Ken Healy
2008-09-15
Hello,

Is anyone aware of the conditions under which buffered-HF (BOE) etching
is diffusion limited, or a reference which discusses this?

The particular situation I'm interested in is etching a 5um thick
silicon dioxide layer at the bottom of a KOH-etched pit in silicon, as
shown below. The silicon is 500um thick and base of the pit (top in the
diagram) is ~ 100um x 100um.


membrane nitride
======================================================================
dielectric oxide               |        |
--------------------------------        ------------------------------
                               /          \
                              /            \
silicon                     /              \
                            /                \
                           /                  \
--------------------------                    ------------------------
mask oxide               |                    |
==========================                    ========================
mask nitride


I have measured the etching rate of my 6:1 BOE solution to be 60nm/min
on fully exposed oxide. I suspect the etching rate in this case may be
diffusion limited due to the geometry, because, after 2h20min the oxide
still does not appear to be fully etched. My doubt is due to the fact
that it is hard to measure the the actual thickness in this case. All I
have to go on are SEM images showing undercut, which suggests at least
some etching, and TEM observations where the electron beam is scattered
so much it is impossible to focus the beam at high magnifications.

Regards,

Ken Healy

Dept of Physics and Astronomy
University of Pennsylvania

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing