MEMSnet Home: MEMS-Talk: How to cut thin ZnO foil without damaging surface roughness and without deformation!
How to cut thin ZnO foil without damaging surface roughness and without deformation!
2008-09-16
alim polat
2008-09-16
Krueger, Bernd
How to cut thin ZnO foil without damaging surface roughness and without deformation!
alim polat
2008-09-16
Hello Everyone

I have this thin ZnO thin film foil and I want to cut it to get mm
scale, for example 7 mm x 7 mm without damaging its surface
smoothness. So the two important factors are:
1. Surface should stay smooth. No damage to the surface.
2. Also I don't want to deform the surface when I cut it.
I really appreciate if you give me some suggestions. Thank you very
much. Let's support MEMS-TALK.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing