MEMSnet Home: MEMS-Talk: Re: Spin coating of the THICK PMMA
Re: Spin coating of the THICK PMMA
1998-09-13
Jayant Neogi
1998-09-14
Armin Kuebelbeck
1998-09-30
Skrobis, Ken
Re: Spin coating of the THICK PMMA
Jayant Neogi
1998-09-13
Hi:

If you spin coat a mono-layer of HMDS before you spin coat PMMA it will
take care of your adhesion problem. Here HMDS helps in good adhesion of
PMMA to any substrate. If you need any specific information please feel
free to contact me.

Regards
Jayant Neogi
Director:Norsam Technologies
Ph# 503-640-0586

Oh, Dong-young wrote:

> Good Morning Everyone!
>
> It's morning now in SoutKorea.
> I'm doing a project which using a LIGA process.
> But, I have a problem to make a good adhesion between  the Si
> wafer(3000A Ti layer on) and the thick PMMA sheet.
> Does anybody know how to make a 100um PMMA using a spin coating
> technique?
> or make a strong adhesion between the PMMA sheet and the wafer??
>
> Thanks!
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation