MEMSnet Home: MEMS-Talk: SU-8 delamination problem
SU-8 delamination problem
2008-10-23
Dhananjay Dendukuri
2008-10-23
Bruce Altemus
2008-10-23
Gareth Jenkins
2008-10-23
Eric Johnston
2008-10-23
Jian Wang
2008-10-23
Bill Moffat
2008-10-24
Meifang Lai
2008-10-24
Gareth Jenkins
2008-10-25
Dendukuri
2008-10-23
Michael Larsson
SU-8 delamination problem
Dendukuri
2008-10-25
Dear All,

Thanks for the many relevant and useful replies.  We are trying with high
exposure times first and I will let you know once (if!) we solve the
problem.

Best,
Dhananjay

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation