MEMSnet Home: MEMS-Talk: How to deposit Tungsten blanket on Oxide layer
How to deposit Tungsten blanket on Oxide layer
2008-10-10
Pothisorn, Araya - potay006
2008-10-10
Kirt Williams
2008-11-14
Henn, Gudrun: Ms.
How to deposit Tungsten blanket on Oxide layer
Henn, Gudrun: Ms.
2008-11-14
Hi,

sputtering tungsten is surely the choice. If you can adjust stress you even can
leave the adhesion layer and get working results.

Regards,

lumina


-----Ursprüngliche Nachricht-----
Von: [email protected] [mailto:[email protected]] Im
Auftrag von Pothisorn, Araya - potay006
Gesendet: Freitag, 10. Oktober 2008 05:42
An: [email protected]
Betreff: [mems-talk] How to deposit Tungsten blanket on Oxide layer

Hi all,

I'm new in MEMS. Does anyone have experience in deposit tungsten on
Oxide layer? I need to deposit 1000 angstorm of tungsten blanket on the
oxide layer.

Regards,

Araya
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics