MEMSnet Home: MEMS-Talk: Double lithography problem with SU1828-TI35ES
Double lithography problem with SU1828-TI35ES
2009-01-29
basar bolukbas
2009-01-29
Bill Moffat
2009-01-30
basar bolukbas
2009-01-30
Bill Moffat
2009-01-30
basar bolukbas
2009-01-30
Edward Sebesta
2009-01-30
basar bolukbas
2009-02-02
Edward Sebesta
Double lithography problem with SU1828-TI35ES
basar bolukbas
2009-01-30
Hello Bill,

Thank you very much for your answer.

What you mean you said ''Silylate''.
How can i set to Silicon barrier? Do you you mean SiN deposition?
If so i can deposite with PECVD-Sputtering.

Best Regards.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.