A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Double lithography problem with SU1828-TI35ES
Double lithography problem with SU1828-TI35ES
2009-01-29
basar bolukbas
2009-01-29
Bill Moffat
2009-01-30
basar bolukbas
2009-01-30
Bill Moffat
2009-01-30
basar bolukbas
2009-01-30
Edward Sebesta
2009-01-30
basar bolukbas
2009-02-02
Edward Sebesta
Double lithography problem with SU1828-TI35ES
Edward Sebesta
2009-01-30
Silayte means to treat with a silicon containing vapor which reacts with
the polymer silayting it. Thus the polymer will have silicon in it, or
at least at the surface.

Ed

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of basar bolukbas
Sent: Friday, January 30, 2009 12:11 AM
To: mems litho
Subject: Re: [mems-talk] Double lithography problem with SU1828-TI35ES


Hello Bill,

Thank you very much for your answer.

What you mean you said ''Silylate''.
How can i set to Silicon barrier? Do you you mean SiN deposition?
If so i can deposite with PECVD-Sputtering.

Best Regards.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation