A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Aluminum wedge bonding from substrate to die
Aluminum wedge bonding from substrate to die
2009-02-24
GARCIA BLANCO Sonia
2009-02-24
Adamson, Steve
Aluminum wedge bonding from substrate to die
Adamson, Steve
2009-02-24
If I understand your question, you are just reversing the order of the
bonds. It sounds like it should work fine.


Regards,
Steven J. Adamson
Market Manager, Asymtek
First Past President IMAPS

Device Packaging Conference
Global Business Council
March 8-12, 2009
Scottsdale , AZ
www.imaps.org/devicepackaging

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of GARCIA BLANCO Sonia
Sent: Tuesday, February 24, 2009 12:47 PM
To: General MEMS discussion
Subject: [mems-talk] Aluminum wedge bonding from substrate to die

Hi,

Hopefully you can help me!

We normally do aluminum wedge bonds from die to substrate and it works
very well. However, due to the mechanical limitations on a current
package on which we are currently working on, we were considering having
to bond from substrate to the IC die. Is there any norm or design rule
that does not permit doing so?

I would really appreciate if you could give me some advice on that!

I am looking forward to your feedback,

Have a very nice day!

Sonia Garcia Blanco, PhD
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMStaff Inc.