[email protected]
Hard baking. Adhesion. RE: definition of hard bake and hard bake recipes
2009-02-25
Edward Sebesta
2009-02-28
Evelyn B
2009-02-28
Edward Sebesta
2009-02-26
Robert Black
definition of hard bake and hard bake recipes
Robert Black
2009-02-26
A hard bake is simply a bake after the develop step. It is not the same as a
UV bake (which is done in a uv bake tool).  The hard bake temp depends on
the resist you are using. (for i-line it is about 110-125). Reflow is when
you bake over its glass temperature (about 160) and the pac starts to
breakdown and the resist "melts".

If you UV bake and crosslink the resist you can bake at temps over 160 and
still keep the original profile.

Robert

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of [email protected]
Sent: Wednesday, February 25, 2009 1:39 PM
To: [email protected]
Subject: [mems-talk] definition of hard bake and hard bake recipes

Hello all,

I was looking for the definition of "hard bake" to enhance
substrate-photoresist interface during wet etch processes. I found
that there is no exact definition for that.

Some of the users simply keep their developed PRs at elevated
temperatures and call this "hard bake" while some other users use
"UV-curing tools" to cure their PRs before keeping their PRs at
elevated temperatures for extended time, or some others use a
convection oven to hard bake their PRs.

 From here I understand that the definition is not very important as
long as the final result is successful... But from my experience, I
know that keeping the PR at elevated temperatures is simply called
"reflow" but not "hard bake".

My question is that:

What recipe should I use to enhance my silicon-PR interface for ~90
minutes of BOE (6:1) etch?

I am thinking about modifying my mask, but before starting that I want
to see what I can do with the example that I have in my hands. This
way it will be much cheaper, and if there is a solution, it will
definitely be much faster than modifying my masks and doing everything
from scratch...

I have several PR options, which are:

SPR220-3.0,
SPR700-1.2L,
SPR955-CM 0.9, or
SPR955-CM 2.0

Is there somebody who used one of those PRs, and achieved a good
adhesion against BOE(6:1) etch for extended etch time (~90 minutes).

Best regards,

Mehmet Yilmaz
Mechanical Engineer
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing