Glass cracking after anodic bonding
2009-03-17
Mehmet Aykol
2009-03-20
Brubaker Chad
Glass cracking after anodic bonding
Mehmet Aykol
2009-03-17
Hi all,Few weeks ago someone else asked about glass cracking after anodic
bonding. I am having the same problem but form a different reasons. My
cracks seem to nucleate form the holes I drilled using a diamond drill bit
(3/4mm) attached to a Dremmel. The cracks start after I start cooling down
the device. I ramp down the temperature as well. My bonding conditions are
500C and 700V. I am using a spring loaded gold pin as the top electrode. How
can I avoid these cracks?

--
Mehmet Aykol
University of Southern California
EE - Electrophysics
Phone: (213) 821-4090
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
MEMS Technology Review
Process Variations in Microsystems Manufacturing