Hi all,

In reviewing my process flow using Coventorware I have noticed some aspect
ratios that seem quite low.  They vary from 0.25 and can get as low as
0.01.  Can anyone provide a good rule of thumb for an aspect ratio using wet
processes?

Thanks,

Evelyn

--
EVELYN BENABE
Graduate Research Assistant
RF Microsystems Research Group
University of South Florida
4202 East Fowler Avenue
Tampa, FL 33620
Office: ENB 412
Office Phone: (813)-974-4851
Email: [email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.