Hello,

If this is just a temporary fixture, you may be able to use
photoresist to glue the backside of your silicon wafer to your glass
disk.  If you get to a point in which you don't need the glass disk
anymore, you should be able to remove the resist using acetone to
unglue your Si wafer from the glass disk.  Hope this helps.

Tony P

On Thu, May 7, 2009 at 9:43 AM, Maria Matschuk
 wrote:
> Dear all,
>
> I need to fix a Silicon wafer (coated with resist) to a glass disk. Does
anyone have experience with some kind of glue (or another method)?
>
> Kind Regards
>
> Maria

--
Tony Price
Department of Electrical Engineering
University of South Florida
4202 E. Fowler Avenue, ENB-118,
Tampa, FL, 33620
Office: ENG 108
Phone: (813) 396-9310
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.