wafer bonding warpage
2009-06-27
杜 彦召
2009-06-28
Yoshi.Sakata_Gmail
2009-06-28
Bill Moffat
2009-06-30
Brubaker Chad
wafer bonding warpage
杜 彦召
2009-06-27
Hi all:
i am bonding one glass wafer and one silicon wafer with epoxy and their TEC is
the same. But why does it have near 500um warpage after bonding?

Thank you!