MEMSnet Home: MEMS-Talk: Gold peel off with PMMA mask
Gold peel off with PMMA mask
2009-08-18
luhaorice
2009-08-18
Ruiz, Marcos Daniel (SENCOE)
2009-08-19
luhaorice
2009-08-19
Ruiz, Marcos Daniel (SENCOE)
Gold peel off with PMMA mask
Ruiz, Marcos Daniel (SENCOE)
2009-08-19
In that case, it seems that the etchant is causing PMMA to lose
adhesion.

Dan

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of luhaorice
Sent: Wednesday, August 19, 2009 11:56 AM
To: General MEMS discussion
Subject: Re: [mems-talk] Gold peel off with PMMA mask

Thanks for your reply.  We didn't open windows near every fine lines.
We also have peel off problem at areas far away (hundreds of microns)
from the windows (rectangle about 1um by 10um).

Thanks,
Hao

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Addison Engineering
Harrick Plasma, Inc.