renil kumar
2009-08-30
Yongliang Yang
gold as electrical contact
Yongliang Yang
2009-08-30
Gold atoms can move into the silicon layer and change the conduction/valence
band structure of silicon (you can find it in any books about semiconductor
physics).

You should employ another layer between Si and Au. The function of this
layer is to  prevent gold atoms from moving into silicon, Usually  Ti, Ti/W,
Cr, Pt are used. Another function is to make sure good contact between
silicon and gold, not only mechanically but also electrically.

In my experience, The Ohmic contact between Ti-Si, Ti/W-Si is good; while
Cr-Si is not as good.



2009/8/30 renil kumar 

> Hi All,
>
>                  Can gold be an electrical contact for n-type SOI wafer. I
> am planning to sputter gold on the SOI wafer as an electrical contact and
> bulk etch the silicon to form the electrostatically movable cantilever. Any
> suggestion would be appreciated.
>
> Thanks in advance.
>
> Renil

--
Yongliang Yang
State Key Lab of Transducer Technology,
Shanghai Institute of Microsystem and Information Technology
Chinese Academy of Science
865 Changning Road Shanghai 200050, P. R. China
Phone: +86 13801756921
E-mail: [email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
University Wafer