MEMSnet Home: MEMS-Talk: Receipe for diluted aqua regia
Receipe for diluted aqua regia
2009-09-15
Christian Engel
2009-09-16
Edward Sebesta
2009-09-16
Gareth Jenkins
2009-09-16
Bob Henderson
Receipe for diluted aqua regia
Edward Sebesta
2009-09-16
Why aqua regia? Why not a KI or NaI solution? You can dilute these
chemistries with ethylglycol or something to slow them further.

Ed

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Christian Engel
Sent: Tuesday, September 15, 2009 3:41 PM
To: [email protected]
Subject: [mems-talk] Receipe for diluted aqua regia


Hi guys,

I want to etch a layer of gold, which has been deposited on a glass
surface, with a thickness of about 30nm by using aqua regia. Non-diluted
the each rate is too strong so I have to relax it a litte bit. Does
anyone have a recommendable receipe for diluted aqua regia? Etch time
should be about 15 seconds for the whole 30nm gold layer...
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
The Branford Group