flowing in rhodamine in pdms channel
2009-09-20
김태진
2009-09-20
Peng Li
2009-09-20
Hong Chen
2009-09-21
Dirk Renckens - TNW
2009-09-20
Depue, Clayton - In-Q-Tel
2009-09-20
amit asthana
flowing in rhodamine in pdms channel
Depue, Clayton - In-Q-Tel
2009-09-20
TJ

PDMS has fairly high
permeability for a lot of fluids and oils, and will leak with time.  You will
probably need to coat with a perfluro compound as a barrier.

Clayton

----- Original Message -----
From: [email protected] 
To: [email protected] 
Sent: Sat Sep 19 20:03:00 2009
Subject: [mems-talk] flowing in rhodamine in pdms channel

Hi all,

I've been trying to flow in fluorescence die (Rhodamine) in a PDMS microfluidic
channel to do some flow characterizations.

The problem is, the vicinity of the pdms channel became bright as well after
about 5 minutes.

It almost seemed like that the fluoresent die was diffused into the pdms.

Is there a way to solve this problem?

Thanks!

TJ
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.