MEMSnet Home: MEMS-Talk: pdms stuck
pdms stuck
2009-11-18
Emanuele Orabona
2009-11-18
Gareth Jenkins
2009-11-19
Emanuele Orabona
2009-11-19
Dirk Renckens - TNW
2009-11-19
Gareth Jenkins
2009-11-20
Emanuele Orabona
2009-11-18
Mikael Evander
2009-11-19
Emanuele Orabona
2009-11-21
amit asthana
pdms stuck
Mikael Evander
2009-11-18
I've used a negative resist stripped called microstrip. When heated to
around 50 C it removes silicone, epoxy and god knows what.

/Mikael

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Emanuele Orabona
Sent: Wednesday, November 18, 2009 1:21 AM
To: [email protected]
Subject: [mems-talk] pdms stuck

Hi all,

Some days ago, I used pdms with a silicon master (with SU-8
structures) to make a microfluidic device. Unfortunately i forgot to
silanize the silicon wafer and some small piece of PDMS stuck on it.
I don't have another master, how can remove completely the pdms?

I've already tried unsuccessfully to clean it with Acetone and
Isopropyl alcohol.

Can you help me?
Thank you
Emanuele
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics