HD offer a variety of Polyimide thinners, failing this using NMP is a
solution.  Bill Moffat

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of James Paul Grant
Sent: Wednesday, January 06, 2010 3:39 AM
To: General MEMS discussion
Subject: [mems-talk] Dilution of Polyimide

Hello all,

Has anyone got an experience of diluting polyimide or more specifically
polyimide from HD Microsystems?

Thanks,

James
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
The Branford Group
Mentor Graphics Corporation