MEMSnet Home: MEMS-Talk: ProteK B3 coating layer removal
ProteK B3 coating layer removal
2010-04-02
Xiaoyong Liu
2010-04-06
Kuijpers, Peter
2010-04-03
Paul Nguyen
2010-04-04
Xiaoyong Liu
2010-04-06
Matthew Koch
ProteK B3 coating layer removal
Kuijpers, Peter
2010-04-06
Goodmorning Xiaoyong,

If your features are covered with SiN, why do you still need Protek for KOH
protection?
In here we  have very good results with Parylene as KOH protection. Removal of
this is done in a O2 plasma
for about 45 min.

best regards,

Peter Kuijpers
MiPlaza Technology Laboratories
Philips Research Europe
High Tech Campus 04
Postbox HTC-4-1
5656 AE Eindhoven
The Netherlands
Tel.: +31 402743667
         +31 612507027
Email: [email protected]


-----Original Message-----
From: [email protected] [mailto:mems-
[email protected]] On Behalf Of Xiaoyong Liu
Sent: Friday 2 April 2010 20:22
To: [email protected]
Subject: [mems-talk] ProteK B3 coating layer removal

Hi,
    I am using a so-called Protek B3 layer (spin coated) from Brewer Sciences as
a protecting layer for my wafer frontside during KOH wet etching. It serves its
purpose pretty well, but it is very hard to remove. I tried the remover (Protek
remover 100) they suggested as well as acetone overnight.

There is still an apparent layer there after overnight soaking in above
solutions. I also tried to use O2 plasma (as well as CF4/O2 combination), but
with no apparent effect.  I am wondering if someone has any experience with it,
and would share their insight with me. By the way, my sample is on Si substrate
coated with a thin layer of SiN. The features are just metal.

Thanks

Xiaoyong

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

The information contained in this message may be confidential and legally
protected under applicable law. The message is intended solely for the
addressee(s). If you are not the intended recipient, you are hereby notified
that any use, forwarding, dissemination, or reproduction of this message is
strictly prohibited and may be unlawful. If you are not the intended recipient,
please contact the sender by return e-mail and destroy all copies of the
original message.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review