A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: PDMS fine structures
PDMS fine structures
2010-12-12
DEBASHIS MAJI
2010-12-13
Gareth Jenkins
2010-12-13
[email protected]
2010-12-14
Michael Cooke
2010-12-14
DEBASHIS MAJI
2010-12-14
Bill Moffat
2010-12-15
Tsoll Doiiu
2010-12-22
DEBASHIS MAJI
PDMS fine structures
DEBASHIS MAJI
2010-12-14
Dear All,

Thanks for your comments and suggestions. Actually I dont have either silane
or the teflon coating with me. I'll try to get them and see. Meanwhile I
shall try to reduce the baking temp of PDMS and check out...

Do you all suggest to clean up the Su8 master after each moulding process
with some chemicals or ultrasonication?

Please advise.
Thanks in advance.

Debashis Maji

On Tue, Dec 14, 2010 at 9:02 PM, Michael Cooke wrote:

> Have you tried a thin telfon layer, or perhaps poorly adhesive metal ?

--
Debashis Maji,
SRF - Texas Instruments & IIT Kharagpur collaborative Project,
PhD Scholar - School of Medical Science & Technology,
IIT Kharagpur, India - 721302
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Addison Engineering
MEMS Technology Review